Micro LED display
Micro LED display
Micro LED technology has surpassed the limitations of OLED, with higher brightness and saturation. In addition, OLED materials are organic light-emitting diodes, which naturally cannot be compared with organic light-emitting diodes such as Micro LED in the service life. Micro LED is more competitive in the application fields requiring the use of time, such as car head-up display and large screen projection. Vacuum plasma in oxygen and nitrogen and add less vacuum plasma in oxygen and nitrogen and add a small amount of carbon tetrachloride, under the condition of discharge, can quickly etch off epoxy resin. 3. Will vacuum plasma completely destroy epoxy resin? Because of the gap between the Mini LED and the surface of the Mini LED, the epoxy resin has a poor thickness, so the vacuum plasma will preferentially etch the epoxy resin on the surface of the Mini LED chip.
Box/yellow light CELL
Box/yellow light CELL
In the whole process of LCD/TFT and other display modules, plasma equipment is used for surface activation and modification many times in the process of box forming/yellow light CELL, which greatly improves the stability of the process.
ITO pretreatment before coating
ITO pretreatment before coating
Plasma cleaning machine treatment can improve the surface topography of ITO better, and it can be seen that the oxygen holes on the surface of ITO increase significantly, and a layer of negatively charged oxygen is enriched on the surface to form an interface dipole layer, which increases the surface work function of ITO and greatly enhances the hole injection ability of ITO. In addition, after the treatment of plasma cleaning machine, the surface roughness of ITO is reduced, the interface between ITO film and NPB can be reduced, the hole injection becomes easier, and the electron injected by the cathode is better combined to generate excitons, and the device prepared by the anode after plasma treatment has high brightness and good quality.
ACF-FPC cable bonding
ACF-FPC cable bonding
After the gold finger is cut by the Laser of the flexible plate, black carbide will appear on the edge, micro-short circuit will be generated in the high pressure test, and detachment phenomenon will occur at high temperature, which seriously affects the reliability and stability of the product and greatly reduces the quality of the product. Using OKSUN low-temperature plasma technology can completely remove black carbides and other pollutants on the molding edge, form a large number of active groups on the surface, serious pressing reliability, eliminate short circuit phenomenon.
COG display chip binding
COG display chip binding
In the COG process of installing bare chip IC on the glass substrate (LCD), when the chip is bonded and hardened at high temperature, the substrate coating composition on the surface of the bonding filler is analyzed. There are also cases where Ag slurry and other connectors overflow and contaminate the bonding filler. If these contaminants can be removed by plasma cleaning prior to the hot pressing binding process, the quality of the hot pressing binding can be greatly improved. Furthermore, as the wettability of substrate and bare chip IC surfaces is improved, the bonding and densivity of LCD-COG module can also be improved, and the problem of line corrosion can be reduced.
  • 微信客服

  • Online

  • Tel

  • 短信咨詢

  • 微信掃碼咨詢

    主站蜘蛛池模板: 网友自拍视频在线观看 | 日韩黄色免费在线观看 | 免费操视频| 亚洲成色WWW久久网站夜月 | 日本欧美一区二区三区在线观看 | 大胆欧美熟妇xxbbwwbw高潮了 | 午夜影院黄色 | 亚洲精品久久久久久久小说 | 欧美丰满熟妇乱XXXXX视频 | 久久久久久久久久久视频 | 一区二区成人在线观看 | 女18一级大黄毛片免费女人 | 四虎院影wwwf678com| 国产成人a亚洲精品 | ag影院免费区 | 亚洲精品第一国产综合精品99 | 噜噜噜综合亚洲 | 91综合中文字幕乱偷在线 | 在线免费av片 | 视频一区中文字幕国产 | 亚洲国产第一站精品蜜芽 | 大学生不戴套毛片视频 | 无码人妻精品丰满熟妇区 | 色综合天天综合高清网 | 精品国精品国产自在久国产应用男 | 18禁男女污污污午夜网站免费 | 一区二区三区无码在线观看 | 日韩在线中文高清在线资源 | 在线播放国产不卡免费视频 | 国产精品原创巨作AV女教师 | 综合精品影视国产 | 九九香蕉视频 | 日韩亚洲欧美中文高清在线 | 久久大香萑太香蕉AV黄软件 | 成午夜免费视频在线观看 | 欧美日韩中文字幕精品 | 97se狠狠狠综合亚洲狠狠 | 久久国产精品波多野结衣AV | 日本三极| 午夜肉伦伦影院无码 | 中文字幕伦乱 |